Vui lòng dùng định danh này để trích dẫn hoặc liên kết đến tài liệu này: http://thuvienso.vanlanguni.edu.vn/handle/Vanlang_TV/18853
Toàn bộ biểu ghi siêu dữ liệu
Trường DCGiá trị Ngôn ngữ
dc.contributor.authorMa, Zhiming-
dc.contributor.authorBa, Guangzhong-
dc.contributor.authorDuan, Zhenhua-
dc.date.accessioned2020-06-02T03:53:21Z-
dc.date.available2020-06-02T03:53:21Z-
dc.date.issued2019-
dc.identifier.issn1687-8086-
dc.identifier.issn1687-8094 (eISSN)-
dc.identifier.otherBBKH1145-
dc.identifier.urihttp://thuvienso.vanlanguni.edu.vn/handle/Vanlang_TV/18853-
dc.description"Hindawi Advances in Civil Engineering Volume 2019, Article ID 2465940, 13 pages https://doi.org/10.1155/2019/2465940"vi
dc.description.abstractConcrete structure is frequently subjected to the fire attack, whereas the permeability of concrete with fire-damage has received little consideration. This paper aims to investigate the chloride permeability of plain concrete and recycled aggregate concrete (RAC) with fire-damage, and the effects of various cooling patterns and recuring treatment on the chloride permeability are also studied. The results manifest that the elevated temperatures result in an increase in the fire-damage and chloride permeability of concrete, and that the increase becomes more obvious with the temperature above 400°C. Attributing to the water-cooling which provides a recuring environment, the chloride permeability after water-cooling is lower than that after air-cooling when the temperature is 200°C. Whereas when the temperature is above 400°C, the chloride permeability after water-cooling becomes higher than that after air-cooling, due to an extra damage that the water-cooling produces. The recuring treatment can reduce the chloride permeability of concrete with fire-damage, and the reduction becomes more significant when the concrete suffers a serious fire-damage. Exposing to the same condition of high temperature, the addition of recycled aggregate (RA) further boosts the fire-damage and chloride permeability of concrete. Particularly, the chloride permeability increases with the increasing of RA replacement ratios, linearly, and the increased temperatures further lead to an increase in the slope of the fitting straight line.vi
dc.language.isoenvi
dc.publisherHindawi Limitedvi
dc.subjectMechanical propertiesvi
dc.subjectConstructionvi
dc.subjectChloridevi
dc.subjectCoolingvi
dc.subjectPermeabilityvi
dc.subjectConcretevi
dc.subjectCooling effectsvi
dc.subjectCeramic fibersvi
dc.subjectConcrete structuresvi
dc.subjectWater damagevi
dc.subjectCivil engineeringvi
dc.subjectCementvi
dc.subjectHigh temperaturevi
dc.subjectReinforced concretevi
dc.subjectFire damagevi
dc.subjectConcrete aggregatesvi
dc.subjectAggregatesvi
dc.subjectHigh temperature effectsvi
dc.subjectStraight line fittingvi
dc.titleEffects of High Temperature and Cooling Pattern on the Chloride Permeability of Concretevi
dc.typeOthervi
Bộ sưu tập: Bài báo_lưu trữ

Các tập tin trong tài liệu này:
Tập tin Mô tả Kích thước Định dạng  
BBKH1145_TCCN_ Effects of High Temperature.pdf
  Giới hạn truy cập
Effects of High Temperature and Cooling Pattern on the Chloride Permeability of Concrete3.74 MBAdobe PDFXem/Tải về  Yêu cầu tài liệu


Khi sử dụng các tài liệu trong Thư viện số phải tuân thủ Luật bản quyền.