Vui lòng dùng định danh này để trích dẫn hoặc liên kết đến tài liệu này: http://thuvienso.vanlanguni.edu.vn/handle/Vanlang_TV/18470
Toàn bộ biểu ghi siêu dữ liệu
Trường DCGiá trị Ngôn ngữ
dc.contributor.authorChen, Liang-
dc.contributor.authorMao, Xianbiao-
dc.contributor.authorYang, Shengli-
dc.contributor.authorChao, An-
dc.contributor.authorWu, Peng-
dc.date.accessioned2020-05-29T05:19:39Z-
dc.date.available2020-05-29T05:19:39Z-
dc.date.issued2019-
dc.identifier.issn1687-8086-
dc.identifier.issn1687-8094 (eISSN)-
dc.identifier.otherBBKH1192-
dc.identifier.urihttp://thuvienso.vanlanguni.edu.vn/handle/Vanlang_TV/18470-
dc.descriptionAdvances in Civil Engineering; New York Vol. 2019, (2019). DOI:10.1155/2019/2375276vi
dc.description.abstractThe coupling effect of freeze-thaw (F-T) temperature and dynamic load on the dynamic mechanical properties and fracture mechanism of saturated yellow sandstone was experimentally investigated in this research. The dynamic compression tests on the specimen after different F-T temperatures (i.e., −5°С, −10°С, −15°С, −20°С, −30°С, and 20°С) have been carried out with split-Hopkinson pressure bar (SHPB) setup under eight F-T cycle numbers. The density and P-wave velocity of the specimens were obtained before and after the F-T tests. After the F-T tests, the specimen microstructures were examined via the scanning electron microscope (SEM). The dynamic fracture process was visualized by the high-speed camera. The particle size distribution and fragment shapes of the specimens were analyzed using a classifying screen. In addition, the energy dissipation law of specimens during the impact test was also discussed. Experimental results show that the dynamic elastic modulus, strength of the specimen, and the average particle size decrease with decreasing F-T temperature. SEM results reveal that low F-T temperature leads to severer internal damage of the specimen by inducing freeze-swell holes, interconnected cracks, and pore clusters. In addition, the fragmentation shapes of the failed specimens exhibit double-cone failure, single-side slope failure, double-side slope failure, and split failure. The energy dissipation increases gradually with increasing F-T temperature. This study helps to prevent geological disasters and optimize engineering design in cold regions.vi
dc.language.isoenvi
dc.publisherHindawi Limitedvi
dc.subjectMechanical propertiesvi
dc.subjectColdvi
dc.subjectImpact testsvi
dc.subjectCompression testsvi
dc.subjectStress-strain curvesvi
dc.subjectSandstonevi
dc.subjectDisastersvi
dc.subjectNonferrous metalsvi
dc.subjectMechanicsvi
dc.subjectFracture mechanicsvi
dc.subjectStorage modulusvi
dc.subjectDynamic loadsvi
dc.subjectHigh speed camerasvi
dc.subjectDesign engineeringvi
dc.subjectTemperaturevi
dc.subjectFailurevi
dc.subjectEnergy dissipationvi
dc.subjectCivil engineeringvi
dc.subjectStonevi
dc.subjectDesign optimizationvi
dc.titleExperimental Investigation on Dynamic Fracture Mechanism and Energy Evolution of Saturated Yellow Sandstone under Different Freeze-Thaw Temperaturesvi
dc.typeOthervi
Bộ sưu tập: Bài báo_lưu trữ

Các tập tin trong tài liệu này:
Tập tin Mô tả Kích thước Định dạng  
BBKH1192_TCCN_Experimental Investigation on ....pdf
  Giới hạn truy cập
Experimental Investigation on Dynamic Fracture Mechanism and Energy Evolution of Saturated Yellow Sandstone under Different Freeze-Thaw Temperatures7.24 MBAdobe PDFXem/Tải về  Yêu cầu tài liệu